Coating equipment spraying reason and processing method of foaming:
The reason:
1 coated surfaces wet or acid, salt, salt and other substances.
2 paint and thinner mixed with water.
3 coated surface is too rough, to absorb a large quantity of paint, coating is too thin.
4 site environmental humidity is big, more than 90%, coating is extremely easy to white light loss.
5 live at too low a temperature, drying too slowly, water gathered in the surface caused by the loss of light.
6 air compressor in the moisture is not removed, mixed with the lesions produced in the coating.
7 excessive amount of diluent.
Solution:
1 clean up by impurity coated surface.
2 take good care of paint, prevent mixing water.
3 note the sanding thickness, guaranteed to be coated pages flat.
4 adjust the indoor temperature or stop construction.
5 construction environment in general the temperature above 10 degrees.
6 remove the air compressor in the gas water, maintenance of oil-water separator.
7 adjust the construction ratio.